    富美家防火板的耐熱、耐磨、耐刮、耐感染、抗沖擊、防水等各項性能相對與其他的表面裝飾材料有突出的優(yōu)勢,所以在市場中的購買前景不錯,下面就來講講生產防火板時候容易出現三個問題,做好預防措施。
    The heat resistance, abrasion resistance, scratch resistance, infection resistance, impact resistance, water resistance and other properties of Fumeijia fire-proof board have outstanding advantages compared with other surface decoration materials, so the purchase prospect in the market is good. Now let's talk about three problems that are easy to occur in the production of fire-proof board, and take preventive measures.
    一、板面局部有白花
    1、 There are some white flowers on the board surface
    產生的原因:
    Causes:
    1、表層紙含膠量不足或干燥中局部樹脂固化
    1. Insufficient glue content of surface paper or partial resin curing during drying
    2、表層紙揮發(fā)物含量過低
    2. The volatile content of surface paper is too low
    3、熱壓式壓力不均勻
    3. Uneven hot pressing pressure
    4、忖墊材料無彈性
    4. The cushion material is inelastic
    5、不銹鋼板表明不平
    5. Stainless steel plate indicates unevenness
    6、樹脂反應過老,分子太大,樹脂流動性大
    6. The resin reaction is too old, the molecule is too large, and the resin fluidity is large
    解決的方法:
    Solution:
    1、提高表層紙樹脂含量或控制干燥溫度,防止局部樹脂固化
    1. Increase resin content of surface paper or control drying temperature to prevent local resin solidification
    2、提高表層紙的揮發(fā)物含量
    2. Improve the volatile content of surface paper
    3、檢修熱壓機,改進加壓面的均勻性
    3. Overhaul the hot press and improve the uniformity of the pressure surface
    4、定期更換忖墊材料
    4. Replace the cushion material regularly
    5、不銹鋼板定期拋光
    5. Regular polishing of stainless steel plate
    6、樹脂應分析檢驗,不合格指標要求時停止使用
    6. The resin shall be analyzed and inspected, and it shall not be used when it is unqualified
    在生產防火板的過程中易出現的問題
    Problems easy to occur in the production of fireproof boards
    二、板面有濕花(水汽),邊緣較為嚴重
    2、 There are wet streaks (moisture) on the board surface, and the edges are relatively serious
    產生的原因:
    Causes:
    1、浸膠紙干燥后揮發(fā)物含量太高
    1. The volatile content of the impregnated paper is too high after drying
    2、印刷木紋的油墨或染料所用的溶劑不合適
    2. The solvent used for printing wood grain ink or dye is inappropriate
    3、浸膠干燥后的膠膜紙吸濕(回潮)
    3. Moisture absorption (moisture regain) of impregnated and dried adhesive film paper
    解決的方法:
    Solution:
    1、降低浸膠紙干燥后的揮發(fā)物含量
    1. Reducing Volatile Content of Dried Impregnated Paper
    2、調換油墨(染料)用的溶劑
    2. Solvent for changing ink (dye)
    3、注意膠膜紙的存放,一般可用塑料布遮蓋
    3. Pay attention to the storage of adhesive film paper, which can generally be covered with plastic cloth
    在生產防火板的過程中易出現的問題
    Problems easy to occur in the production of fireproof boards
    富美家防火板
    三、裝飾板表面開裂
    3、 The surface of the decorative plate is cracked
    產生的原因:
    Causes:
    1、樹脂反應過嫩,分子太小
    1. The resin is too tender and the molecule is too small
    2、樹脂固化不完全
    2. Incomplete resin curing
    3、表層膠膜紙含膠量太高
    3. The adhesive content of the surface adhesive film paper is too high
    解決的方法:
    Solution:
    1、不合格的樹脂停止使用
    1. Unqualified resin shall not be used
    2、適當提高熱壓溫度或延長熱壓時間
    2. Properly increase the hot pressing temperature or extend the hot pressing time
    3、控制表層膠膜紙的含膠量
    3. Control the glue content of the surface adhesive film paper
    生產防火板時候容易出現三個問題就是以上所講解的內容了,您對此有什么想咨詢的地方或者有采購需求,都可以來我們網站http://www.qq1980.cn看看。
    There are three problems that are easy to occur in the production of fireproof boards. If you have any questions or purchase needs, you can come to our website http://www.qq1980.cn have a look.
    聯系我們

    產品銷售熱線:18660816658

    技術方案咨詢:18560211715

    倉庫地址:山東省濟南市天橋區(qū)金鑫產業(yè)園303倉庫

    九江工廠:九江市江東大道3號

    臺灣新竹工廠:臺灣新竹

    泰國曼谷工廠:泰國曼谷

    關注我們
    山東創(chuàng)圖建筑裝飾工程有限公司 備案號:魯ICP備14019259號-2 網站地圖 XML TXT 魯公網安備37010502002020號

    截屏,微信識別二維碼

    微信號:18660816658